Our high chrome cast iron rolls are centrifugally cast to ensure a robust metallurgical bond. The exact alloying parameters, including critical additions of Vanadium (V), are detailed below:
| Code (代码) | C | Si | Mn | Cr | Ni | Mo | V | Hardness (硬度 HSD) | Tensile (抗拉 N/mm²) |
|---|---|---|---|---|---|---|---|---|---|
| HCr II | 2.90-3.30 | 0.30-1.00 | 0.50-1.20 | 15.01-20.00 | 0.70-2.90 | 0.70-2.90 | 0.00-0.60 | 65-80 | ≥ 350 |
| HCr III | 2.90-3.30 | 0.30-1.00 | 0.50-1.20 | 18.01-22.00 | 0.70-1.70 | 1.51-3.00 | 0.00-0.60 | 75-90 |
* Note: P ≤ 0.10%, S ≤ 0.05% strictly controlled for all grades.